一、 抹灰面層起泡、開(kāi)花、有抹紋
1. 現(xiàn)象:抹罩面灰時(shí)操作不當(dāng),基層過(guò)干或使用不灰膏質(zhì)量不好,容易產(chǎn)生面層起泡和有
抹紋現(xiàn)象,過(guò)一段時(shí)間還會(huì)出現(xiàn)面層開(kāi)花,影響外觀(guān)質(zhì)量。
2. 治理:墻面開(kāi)花有時(shí)需經(jīng)過(guò)一個(gè)多月的過(guò)程,在處理時(shí)應(yīng)待墻面確實(shí)不會(huì)再有開(kāi)花情
況,才可以挖去開(kāi)花處松散表面,重新用膩?zhàn)诱已a(bǔ)刮平,最后噴漿。
二、 板條頂棚抹灰空鼓、開(kāi)裂
1. 現(xiàn)象:在板條方向或板條接頭處有裂縫,抹灰層與板條粘結(jié)不良,產(chǎn)生空鼓甚至脫落現(xiàn)
First, plaster surface blistering, blooming, there are wiping pattern
1. Phenomenon: when the dust wipe overlay improper operation, primary too dry or use poor quality gray paste, prone to blistering and surface
Wipe pattern phenomenon will occur over time surface flowering, affecting the appearance quality.
2. Governance: Wall more than a month after flowering process is sometimes needed, should be in dealing with the wall does not have a blooming love
Situation, digging flower Department can loose surface, re-use putty Zhaobu Calibrating the last spray.
Second, lath plaster ceiling void, cracking
1. Phenomenon: the direction of the lath or strip joints, cracks, plaster lath layer and poor adhesion, resulting in hollowing or loss is